S. No.

Matrix

Linearity

Sensitivity

Respon-se Time

Kmapp
(mM)

Shelf Life

Reference

  1.  

Electrochemically deposited PANI

100-400

0.042 mAmg-1 dL-1

240s

1.94

6 weeks

 

[28]

  1.  

MWNTs

19.3-231.6

0.559µA
cm–2 mM-1 

-

7.71

-

 

[29]

  1.  

MWCNT/Screen Printed
Carbon Electrode

99.5-399

0.0059 mAmg-1 dL-1

-

-

2 months

 

[30]

  1.  

Gold electrode

0-80

0.13 mA/mM

15 s

2.94

-

 

[31]

  1.  

ZnO Nanoparticles

0.001 – 0.5µM

23.7µA/µM

-

4.7

-

 

[32]

  1.  

Chitosan-SnO2 nanocomposite

0.26-10.36 mM

34.7 mAmg-1 dL-1cm-2

-

3.8

12 weeks

 

[33]

  1.  

PANI-(CdS-QD)
Nanocomposite

50-500

2.63 ´ 10-5 mA mg-1 dL-1

20s

0.82

7 weeks

 

Present Work

Table 1: Characteristics of PANI-(CdS-QD) electrode along with those reported in literature for cholesterol detection.