Table.1: Mean bond strengths in MPa, standard deviations and ARI scores. Significant differences (p<0.05) between the bond strength of the three pre-conditioning methods within one bracket type are marked with an asterisk “*”.ARI score for tensile testing: 1 = composite remaining on the enamel, 2 = composite remaining on both sides, 3 = composite remaining on the bracket. The number of samples displaying a certain ARI score is given in parenthesis. |