| A=magnification 500 x; B=magnification 3000 x. C= magnification 3000 x after grinding and H3PO4 treatment. The grooves (↑) caused by the SiC abrasive particles, debonded filler particles (→) and transverse microcracks (←) are clearly visible. |
| Figure 3: SEM image of the composite surface prepared by grinding. |