Figure 2: Pictures of the Ninea Extruded Productsb aTreatments (SS-BT)
: 1=85 rpm-232.5°C, 2=60 rpm-232.5°C, 3=110 rpm-275°C, 4=85 rpm-
275°C, 5=60 rpm-190°C, 6=110 rpm-32.5°C, 7=85 rpm-190°C, 8=110 rpm-
190°C, and 9=60 rpm-275°C. bSS=Screw Speed, BT=Barrel Temperature,
and RPM=Revolutions Per Minute.