Month Weight loss in % Contact angle
Initial sample - 83±0.76°
After 2 months 0.60±0.2 80±0.70°
After 4 months 6.93±2.2 76± 1.56°
After 6 months 17.00±1.9 70±2.02°
Table 2: Effect of fouling on contact angle and gravimetric weight loss of starch blended HDPE immersed for a period of 6 months at Ennore port.