Samples |
TG |
|
Temperature of Occurrence |
Step Weight Loss in %
(at respective temperatures) |
Pure LDPE [17,18] |
400-460°C |
One step steep weight loss |
LDPE + Consorita I [17] |
61°C
200°C |
5.33%
9.47% |
LDPE + Consortia I +NBT [17] |
60°C
200°Cs
274°C
380°C |
3.88%
9.01%
11.32%
14.34% |
LDPE + Consortia I + Fullerene 60 nanoparticles [18] |
126°C-155°C
230°C |
12.5%
15.7% |
LDPE + Consortia I + SPION [5] |
98.1°C
112°C
130°C
Above 200°C |
1.9%
4.4%
5.2%
8% |