Figure 3:
XRD patterns of the original stainless steel powder and the PSS hollow fiber membranes sintered at 1050°C under different atmospheres (impurity phases: ∗ Mo
12
Fe
22
C
10
; ◊ Mo2C; ♥ Fe
2
O
3
).