Figure 7: DSC trace for ipp isothermal crystallized from the melt at a- 125°C for one hour then heated to 200°C at scan rate 10°Cmin-1 b-125°C for one hour then annealed at 155°C for one hour then heated to 200°C at scan rate 10°Cmin-1.