Figure 2:
Effect of TiO
2
loading on DNB degradation, C0=50 mg DNB/L. (+) Neat solution;
0.4 mg/mL TiO
2
;
1.0 mg/mL TiO
2
;
1.5 mg/mL TiO
2
; (x) Data estimated from Priya [8].