Sample

[η] (dL/g)

Mn (Da)

Mw/Mn

Τm (oC)

Tg (oC)

Tcc (oC)

ΔHm (J/ g)

Xc* (%)

PPAd-0.20

0.22

5000

2.06

45.0

-53.9

3.0

48.1

52.3

PPAd-0.38

0.38

9000

2.25

45.2

-51.4

2.8

47.3

48,7

PPPim

0.71

19 000

2.22

44.8

- 64.3

- 29.8

53.7

29.1

Xc* WAXD measurement
Table 1: Intrinsic viscosity [η], average molecular weight (Mn), melting point (Τm), glass transition temperature (Tg), cold-crystallization temperature (Tcc), heat of fusion (ΔHm) and degree of crystallinty (Xc) for the aliphatic polyesters used in this study