Sample
Relative density (%)
Hardness (HRB)
Tensile strength (MPa)
Elongation (%)
Fe-1.0 wt% Y2O3 (cold press sintering)
83.35
64.3
379.0
4.5
Fe-1.0 wt% Y2O3 (hot press sintering)
92.0
84.3
518
4
Fe-1.0 wt% Y2O3 (SPS)
95.0
91.2
536.7
2.0