DTG |
DTA |
Pure LDPE [17,18] |
°C |
mg/min |
°C |
μJ/mg |
451 |
1.79 |
107
457 |
129
53 |
LDPE + Consorita I [17] |
56
205 |
0.2116
0.0714 |
58
207,248
362 |
143
120
5.03 |
LDPE + Consortia I + NBT [17] |
56
190
273
368 |
0.1423
0.0367
0.0384
0.0185 |
47
117
144
222 |
22.5
13.3
44.8
135 |
LDPE + Consortia I + Fullerene 60 nanoparticles [18] |
144°C
220°C |
0.3220
0.0500 |
146°C
221°C |
0.167
0.115 |
Where, in the case of Fullerene 60, the first step was recorded as rapid and second step as steady. Consortium I gave better results with both NBT and Fullerene 60 [16,18]. |
LDPE + Consortia I + SPION [5] |
44°C
110°C
144°C
218°C |
0.048
0.052
0.221
0.050 |
46°C
113°C
145°C
222°C |
18.3
12.5
100
90.2 |
|