Figure 2: SEM images of direct electrodeposition of HA on superhydrophilic VACNT films at two bath temperatures (a-b) 23 and (c-d) 70oC. (b) Details of amorphous phosphate formed at 23ºC and (d) HA crystals formed on superhydrophilic VACNT at 70ºC.