Figure 7:
XRD patterns of the catalysts calcined at different temperatures: (a) Mn
12
/FA-PG, (b) Mn
12
/FA-PG/200°C, (c) Mn
12
/FA-PG/300°C, (d) Mn
12
/FAPG/ 400°C, (e) Mn
12
/FA-PG/500°C and (f) Mn
12
/FA-PG/600°C.