Catalyst 973°K 1023°K 1073°K
Wet-Impregnation CH4 CO2 CH4 CO2 CH4 CO2
10%Ni/5% CeO2-ϒ-
Al2O3
28.1 33.14 60.44 62.44 73.95 86.97
10%Ni/5%ZrO2-ϒ-
Al2O3
34.29 40.42 61.33 64.62 91.61 91.45
Co-precipitation            
10%Ni/5%CeO2-
Al2O3
24.51 27.5 53.05 56.55 71.16 70.55
10%Ni/5%ZrO2-
Al2O3
23.45 30.71 55 56.55 74.61 87.62
Table 4: Effect of Reaction Temperature on CH4 and CO2 Conversion