alexa Nanomechanical characterization of human hair using nanoindentation and SEM.
Environmental Sciences

Environmental Sciences

International Journal of Waste Resources

Author(s): Wei G, Bhushan B, Torgerson PM

Abstract Share this page

Abstract Human hair is a nanocomposite biological fiber with well-characterized microstructures. Nanomechanical characterization of human hair can help to evaluate the effect of cosmetic products on hair surface, can provide a better understanding of the physicochemical properties of a wide variety of composite biological systems, and can provide the dermatologists with some useful markers for the diagnosis of hair disorders. The paper presents systematic studies of nanomechanical properties of human hair including hardness, elastic modulus and creep, using the nanoindentation technique. The samples include Caucasian, Asian and African hair at virgin, chemo-mechanically damaged and treated conditions. Hair morphology was studied using scanning electron microscopy (SEM). Indentation experiments were performed on both the surface and cross-section of the hair, and the indents were studied using SEM. The nanomechanical properties of hair as a function of hair composition, microstructure, ethnicity, damage and treatment are discussed. This article was published in Ultramicroscopy and referenced in International Journal of Waste Resources

Relevant Expert PPTs

Relevant Speaker PPTs

Recommended Conferences

Peer Reviewed Journals
 
Make the best use of Scientific Research and information from our 700 + peer reviewed, Open Access Journals
International Conferences 2017-18
 
Meet Inspiring Speakers and Experts at our 3000+ Global Annual Meetings

Contact Us

 
© 2008-2017 OMICS International - Open Access Publisher. Best viewed in Mozilla Firefox | Google Chrome | Above IE 7.0 version
adwords