alexa Abstract | OPTIMIZATION OF WELD CRACK EXPANSION DEFECT OF WHEEL RIMS BY USING TAGUCHI APPROACH: A CASE STUDY
ISSN ONLINE(2319-8753)PRINT(2347-6710)

International Journal of Innovative Research in Science, Engineering and Technology
Open Access

Like us on: https://twitter.com/ijirset_r
OMICS International organises 3000+ Global Conferenceseries Events every year across USA, Europe & Asia with support from 1000 more scientific Societies and Publishes 700+ Open Access Journals which contains over 50000 eminent personalities, reputed scientists as editorial board members.

Open Access Journals gaining more Readers and Citations

700 Journals and 15,000,000 Readers Each Journal is getting 25,000+ Readers

This Readership is 10 times more when compared to other Subscription Journals (Source: Google Analytics)

Research Article Open Access

Abstract

For off-line quality control, Taguchi realized that the best opportunity to eliminate variation is during the design of a product and its manufacturing process. Consequently, he developed a strategy for quality engineering that can be used in both contexts. Analysis of variance (ANOVA) is uses to analyze the significant factors of weld crack expansion defect of wheel defects of wheel rim manufacturing. This industry is located in northern part of India and producing the wheel rims. The main components manufactured by this firm are the wheel rims of automobiles. The range of diameter of wheel rims ranges from 10 inches to 30 inches and width may vary from 2.25”– 13” (inches). Through the Taguchi parametric design approach, the optimum levels of process parameters are determined. The percentage of contribution of each process parameter is determined by Analysis of variance. Taguchi’s experimental design yielded optimized control factors, resulting in superior product quality and stability. It is concluded that for weld crack expansion defect, the most significant factor is impact force (factor C) out of three factors.

To read the full article Peer-reviewed Article PDF image | Peer-reviewed Full Article image

Author(s): Dr. D. R. Prajapati , Daman Vir Singh Cheema

Keywords

Weld crack expansion defects, wheel rim manufacturing industry, Taguchi approach, ANOVA technique, Aerospace Engineering,Applied Electronics,Applied Sciences,Biomedical Engineering,Botany,Fluid Dynamics.

Share This Page

Additional Info

Loading
Loading Please wait..
 
 
Peer Reviewed Journals
 
Make the best use of Scientific Research and information from our 700 + peer reviewed, Open Access Journals
International Conferences 2017-18
 
Meet Inspiring Speakers and Experts at our 3000+ Global Annual Meetings

Contact Us

 
© 2008-2017 OMICS International - Open Access Publisher. Best viewed in Mozilla Firefox | Google Chrome | Above IE 7.0 version
adwords